Burma Teakwood Board Resolution Method

Consumers understand the Burma Teakwood Board fake three methods can be aware of, but in the purchase of the same time to pay attention to distinguish. The following is a tour of the forest to teach you some way to identify true and false Burma Teakwood Board, most of the resolution method is built on the plate or the back of the block is not on the basis of the seal, if all the paint plus some hands and feet in the process , It is difficult to distinguish.

One, look at the texture

True Burma Teakwood Board has obvious ink lines and oil spots, fake Burma Teakwood Board or no ink lines or ink lines are light and scattered.

Second, personally touch

Really Burma Teakwood Board feels slippery, feel very delicate, as if soaked in oil, fake Burma Teakwood Board is very rough.

Third, smell the smell

The Burma Teakwood Board emits a special scent, and if the teak is large or even the whole hall is teak, it can smell it in the fragrance, and the fragrance smells soothing, and the Burma Teakwood Board is either fragrant or unpleasant The smell;

Four, weigh the weight

True teak floor fiber density of 0.67 to 0.73 / cm3, lighter than rosewood, but heavier than cauliflower, there is a moderate sense, false Burma Teakwood Board is generally heavy.

Five, water test

Drop the water in the Burma Teakwood Board without paint, the real Burma Teakwood Board on the water bead-like distribution will not penetrate; and fake Burma Teakwood Board will be on the water or Burma Teakwood Board dripping test or slow penetration (teak floor is rich in oil , Water and oil are incompatible, so true Burma Teakwood Board water is not absorbed into a bead-like distribution). When wiping the water stains with a paper towel, you will find that the water on the Burma Teakwood Board will not penetrate and the oily surface is smooth and the water will dry up quickly and leave no trace. The Burma Teakwood Board has been infiltrated and the surface is rough , Water stains do not dry, and paper scraps;

Six, see sawdust

In the floor to install the link is better to identify, really Burma Teakwood Board sawdust has a heavy oil, pinch when there is soft feeling, and fake Burma Teakwood Board sawdust is dry and loose;

Seven, water soak

The floor into the water soak for 24 hours after the observation of its changes, without any change is really Burma Teakwood Board; if the distortion, expansion and other deformation of teak health needs sun and rain, then fake Burma Teakwood Board.

Eight, fire burning

With a destructive test, the general store has a Burma Teakwood Board sample, take a small piece of dry floor for burning, really Burma Teakwood Board distributed smoke thick and large, and fake Burma Teakwood Board is less.